HOME > Boat > Boat Rubber Sheet (Hypalon Fabric)
Characteristics of Boat sheet
NH 100 CSM
Base fabric : N66 - 840D
coating : Ext : Chlorosulfonated Polyethylene (CSM)
Int : Polychloroprene (CR)
Specifications | Unit | Direction | Standard-Test | Spec |
---|---|---|---|---|
Thickness | mm | - | KS K 0506:2006 | 0.9 ↑ |
Weight | g/m2 | - | KS K 0514:2006 | 1.000 ↑ |
Tensile Strength | N/5cm | Warp | KS K 0521:2006 C.R.E 3TRIP METHOD |
2.000 ↑ |
Weft | 1.800 ↑ | |||
Resistance to Weather | N/5cm | Warp | KS K ISO 105 B04 2007 |
1.700 ↑ |
Weft | 1.500 ↑ | |||
Tear Strength | N | Warp | KS K 0536:2009 C.R.E TONGUE METHOD |
80 ↑ |
Weft | 80 ↑ | |||
Tensile Strength in Welding Part |
N/5cm | - | KS K 0530:2007 C.R.E |
1.500 ↑ |
Abrastion Resistance | Weight Loss, mg |
- | KS K 0818:2006 taber Method |
500 ↓ |
Colorfastness to Weather |
Grade | - | KS K ISO 105 B04: 2007 |
4 ↑ |
Temperature Cycle | Appearance | - | Ministry of Land, Transport and Maritime Affairs 2004-77 |
NO CHANCE |
Remark |
NH 210 CSM
Base fabric : N66 - 1680D
coating : Ext : Chlorosulfonated Polyethylene (CSM)
Int : Polychloroprene (CR)
Specifications | Unit | Direction | Standard-Test | Spec |
---|---|---|---|---|
Thickness | mm | - | KS K 0506:2006 | 1.1 ↑ |
Weight | g/m2 | - | KS K 0514:2006 | 1.500 ↑ |
Tensile Strength | N/5cm | Warp | KS K 0521:2006 C.R.E 3TRIP METHOD |
4.900 ↑ |
Weft | 4.900 ↑ | |||
Resistance to Weather | N/5cm | Warp | KS K ISO 105 B04 2007 |
3.920 ↑ |
Weft | 3.920 ↑ | |||
Tear Strength | N | Warp | KS K 0536:2009 C.R.E TONGUE METHOD |
392 ↑ |
Weft | 460 ↑ | |||
Tensile Strength in Welding Part |
N/5cm | - | KS K 0530:2007 C.R.E |
3.920 ↑ |
Abrastion Resistance | Weight Loss, mg |
- | KS K 0818:2006 taber Method |
500 ↓ |
Colorfastness to Weather |
Grade | - | KS K ISO 105 B04: 2007 |
4 ↑ |
Temperature Cycle | Appearance | - | Ministry of Land, Transport and Maritime Affairs 2004-77 |
NO CHANCE |
Remark | standard width : 57in - 146 |
NH 310 CSM
Base fabric : Aramide
coating : Ext : Chlorosulfonated Polyethylene (CSM)
Int : Polychloroprene (CR)
Specifications | Unit | Direction | Standard-Test | Spec |
---|---|---|---|---|
Thickness | mm | - | KS K 0506:2006 | 1.0(±10%) |
Weight | g/m2 | - | KS K 0514:2006 | 1,300(±10%) |
Tensile Strength | N/5cm | Warp | KS K 0521:2006 C.R.E 3TRIP METHOD |
15.000 ↑ |
Weft | 8.000 ↑ | |||
Resistance to Weather | N/5cm | Warp | KS K ISO 105 B04 2007 |
14.000 ↑ |
Weft | 7.000 ↑ | |||
Tear Strength | N | Warp | KS K 0536:2009 C.R.E TONGUE METHOD |
550 ↑ |
Weft | 700 ↑ | |||
Tensile Strength in Welding Part |
N/5cm | - | KS K 0530:2007 C.R.E |
8.000 ↑ |
Abrastion Resistance | Weight Loss, mg |
- | KS K 0818:2006 taber Method |
500 ↓ |
Colorfastness to Weather |
Grade | - | KS K ISO 105 B04: 2007 |
4 ↑ |
Temperature Cycle | Appearance | - | Ministry of Land, Transport and Maritime Affairs 2004-77 |
NO CHANCE |
Puncture Resistance | N | - | KS K 0744:2007 C.R.E |
2.,000 ↑ |